Ceramics glazing mistakes aren’t always the end of the world; they can make your piece more unique, or you can even fix them. To catch these issues, focus on the adhesion of the glaze on your piece and how evenly it covers the surface. Make sure you’re not putting the glaze on too thick, and double-check the firing conditions are correct for the glaze and the piece. Unexpected results add character, but safety should come first.
Key Takeaways for Fixing Glazing Mistakes:
- Catch problems before firing, if possible. Checking for uneven glaze coverage, heavy buildup, cracks, and flaking while you still have the chance to correct it can be helpful.
- Focus on adhesion of the ceramics glaze, not just coverage. Adding another coat won’t necessarily fix glaze that’s lifting or peeling.
- Inspect the entire piece, clean unwanted glaze from kiln-contact surfaces, and confirm the appropriate firing conditions before putting the piece into the kiln.
- Identify the issue before choosing how you want to fix it. Different types of issues have various causes and solutions.
- Keep in mind that some ceramics glazing mistakes can make your piece unique and full of character, but it can also be unsafe to use for its original intended purpose.
- Experiment with your pieces, and keep a record of what works and what doesn’t.
Common Glazing Mistakes and How to Spot Them
Mistakes, or “happy accidents” are common, but they are not the end of the world. Most mistakes are easy to correct or even include in your final product.
Uneven or Thick Layers
Uneven or overly thick application on your creation can cause some glaze mistakes. Heavy buildup, thick overlaps, and glaze collecting around handles or carved details are worth checking before firing your piece.
The thick coating can shrink and crack as it dries, so make sure you’re following the application and coverage method that’s recommended for that glaze.
Using a Glaze That Won’t Attach Properly
Cracking, lifting, or flaking in the dried glaze are signs the coating may not remain properly attached to the clay. During firing, separated areas can pull back into islands of glaze, leaving bare patches.
Surface Contamination
Dust or grease on an item that has gone through a first kiln firing can prevent an even fired coating when it goes in the kiln again. Dust or grease can interfere with the adhesion, but a lightly damp sponge can remove surface dust.
Layering Complications
Layering glaze can create potential weak points in your items. If the lower coating is powdery or poorly attached, adding another layer can make the problem worse. Follow tested layering instructions before assuming any two glazes will work well together.
Checking Your Work Before It Goes Into the Kiln
A final inspection of your piece can help prevent some issues with glazing, especially the factors that are easier to control than others.
Inspect the Entire Piece
Turn the piece in good light, look around its handles, inside rims, and along textured areas to spot any issues before putting it into the kiln. Pay close attention to thick accumulations and cracks in the dried coating, as these areas may be at risk for crawling or blistering in the kiln.
Check Contact Surfaces
Make sure to check the surfaces that will touch: the foot of the piece and the kiln shelf. Remove unwanted glaze from areas of your piece that will touch the kiln shelf, as glaze may accidentally fuse your pottery permanently to the kiln shelf.
Address a Weak Coating
Instead of adding more glaze to fix cracked, flaking, or lifting clay, correct the underlying application problem. For visibly cracked or lifted coating, consider washing off the glaze and starting again as opposed to adding another layer.
That added layer may hide the problem without solving it, and the glaze may pull away from those weaker areas during firing, leaving bare patches. Removing the unstable glaze coating, letting the piece dry, and addressing the cause before glazing again could help with the problem!
Allow the Piece to Fully Dry
Build drying time into your process instead of glazing and loading the piece into the kiln in one uninterrupted step. It’s always best practice to allow your glazed work to dry fully before putting it into the kiln.
Check Kiln Firing Conditions
Check the clay and glaze instructions with the kiln operator before putting your piece inside. Have an idea of what temperature is best for your piece and how long it should be in the kiln.
Evaluating Glaze Problems After Firing
If your piece comes out of the kiln and does not look exactly like you had hoped, don’t fret! Start by identifying what you can actually see, then work toward a possible cause of the issue.
Crawling
Crawling happens when the glaze pulls away from parts of the clay, resulting in bare patches that are surrounded by thicker glaze rather than continuous coverage.
Possible reasons for crawling could be poor adhesion, dust or grease, or a coating that cracked during drying. To prevent this, you could clean the piece, adjust application thickness, or look into the glaze’s formulation.
Pinholes
Pinholes are small openings or pits on the surface. They can form when gases escape through the molten glaze and the openings don’t heal before it stiffens.
The clay body, glaze composition, coating thickness, and firing cycle can all be contributing reasons for pinholes. A firing adjustment could help, but firing hotter may not always be the solution.
If you don’t want to refire the piece, you can sand the pinholes with a fine sandpaper. Colors may look slightly altered, but that can also add character to the piece!
Blisters
In ceramics, blisters are bubbles, raised areas, or broken craters that form during firing. They can be caused by trapped gases, glaze that’s too thick, or overfiring.
if your piece has blisters, check for sharp edges in addition to any appearance issues, as a blistered piece could be unsuitable for functional use. A potential fix for blisters on your piece would be to make sure you are applying thin layers of glaze.
Fix It or Embrace the Quirk?
So, your piece didn’t come out exactly like you had hoped. Depending on the situation, the “issue” could actually be a happy accident that adds character to your piece. Sometimes, though, if the problem makes the piece unsafe to use, it might be best to address it or use the piece for a different function.
First, ask yourself: Does the defect comprise the piece? Then, go from there.
An unexpected visual mistake may be worth keeping, and it might even add an unintended uniqueness to the piece. Be careful with loose glaze or sharp edges, as those mistakes should be treated with caution. If the piece would be unsafe to use for its intended purpose, it may need fixing.
For example, a decorative sculpture could still work as a piece if there’s a mistake. But a mug should be treated differently as a mistake could make it unsafe to drink from.
If an unexpected mistake turns into part of the piece that genuinely works, it can become a creative direction instead of a failed attempt! Use your best judgment and creativity when it comes to deciding whether or not to keep the piece for its original intended use.
Lessons From Happy Accidents
Unexpected results become more useful when you can learn what caused it.
Build a studio record for each project with a mistake, keeping track of:
- Glaze names or recipes
- Glaze application method
- Layer order
- Description of the clay body/piece
- Firing schedule
Also note where the mistake appeared (bonus points for adding pictures to your records!)
Keeping a record will help you isolate variables to investigate and keep track of what works and what does not.
Change one variable at a time to get to the bottom of the problem. This will help you identify the cause of the issue and can even be a fun experiment if you go into it with a curious mindset.
Let these happy accidents suggest possibilities without lowering your standards. Some deliberately developed ceramic pieces once began with mistakes that actually led to a better piece.
Frequently Asked Questions About Ceramics Glazing Mistakes:
Can you fix glazing mistakes before firing?
Often, yes you can! A thin or missed area may need more glaze, while a coating that is cracking, lifting, or flaking needs to be addressed. Be sure you’re not adding more glaze to an unstable layer, as this may not improve its attachment to the clay.
Why is my glaze cracking or peeling before it goes into the kiln?
It may be shrinking too much as it dries. An overly thick application can cause cracks, which can be starting points for crawling during firing. These issues are definitely worth addressing before loading the kiln.
Can you reglaze and refire a piece after firing the first time?
Sometimes, but it depends on the issue. Certain surface problems could improve with a carefully chosen firing adjustment, but others might need changes to the glaze or the clay itself. The safe option is to figure out the problem and then decide whether or not another firing is worth it.
Is pottery with flaking glaze safe for food or drinks?
Don’t use pottery with glaze that flakes as dishware. Sharp glaze fragments can shed off and get into the food or drinks.
Call us at 888-838-3625 or email info@clay-king.com for more glazing tips!
Still figuring out where to start? Or, have questions about how to avoid mistakes while glazing? The Clay-King team is here to help. We’ve spent a lot of time thinking about glazes, and we love matching potters to the right products for their projects and skill levels. Give us a call at 888-838-3625 or send us an email at info@clay-king.com and we’ll be happy to point you in the right direction.